The furnace must be luted before you put the metal in it, with earth
from Valenza, and over that with ashes.
[
Footnote 1. 2.: Terra di Valenza.--Valenza is north of
Alessandria on the Po.]
OF RESTORING THE METAL WHEN IT IS BECOMING COOL.
When you see that the bronze is congealing take some willow-wood cut
in small chips and make up the fire with it.
THE CAUSE OF ITS CURDLING.
I say that the cause of this congealing often proceeds from too much
fire, or from ill-dried wood.
TO KNOW THE CONDITION OF THE FIRE.
You may know when the fire is good and fit for your purpose by a
clear flame, and if you see the tips of the flames dull and ending
in much smoke do not trust it, and particularly when the flux metal
is almost fluid.
OF ALLOYING THE METAL.